Powder Production at Athens, AL with Jordan Ralph
![](https://play.vidyard.com/G7oaWYQakmaJvBCQdp2njy.jpg)
Carpenter Additive's Athens AL facility houses Carpenter Technology's largest vacuum atomizer and it is the heart of the process for making additive manufacturing metal powder at Carpenter Additive. The Athens facility is capable of producing up to 18,000lbs of metal powder per day.