Webinar: Comparison of AM Titanium Parts from EIGA and Plasma Atomized Ti64 Powders

In this session, we discuss the results of a recent comparative study where test specimen parts printed by laser powder bed fusion (LPBF) utilizing both EIGA and plasma atomized powders were investigated by comparing their chemical, microstructural, mechanical, and physical properties conducted within the framework of the ASTM F3001 and F3302 standards.